How the battery degradation over years calculation works
- Calendar fade happens even when a battery sits unused: roughly 1%/yr for LiFePO4, 2%/yr for NMC and 2.5–3%/yr for lead-acid.
- Cycle fade assumes each chemistry reaches 80% capacity at its typical rated cycle life.
- Heat speeds up both kinds of fade. Keeping batteries near 20–25°C extends their life.
Frequently asked questions
How long do solar batteries last?
+
LiFePO4 batteries typically last 10–15 years and 3,000–6,000 cycles before dropping to 80% capacity. Lead-acid batteries usually last 3–7 years.
What does 80% state of health mean?
+
The battery can hold 80% of its original capacity. Most warranties define end of life at 60–80%, though the battery still works beyond that.
How can I slow battery degradation?
+
Avoid high temperatures, avoid sitting at 100% charge for long periods, and use moderate depths of discharge where possible.